Universal Wire Works 67 Nickel Alloy Welding Wire

Category Metal , Nonferrous Metal , Copper Alloy , Nickel Alloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 67 Nickel Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy 67 is used for TIG, MIG, oxyacetylene and submerged-arc welding of 70/30, 80/20 and 90/10 copper-nickel alloys, as well as overlaying on steel. On applications using submerged-arc welding, a first layer of Alloy 60 should be used. Dissimilar welding applications of Alloy 67 include: joining nickel 200 and Monel type alloys to copper-nickel alloys.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 345 MPa
50000 psi
Elongation at Break 30 %
30 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.040 %
<= 0.040 %
Copper, Cu >= 65 %
>= 65 %
As Remainder
Iron, Fe 0.40 - 0.70 %
0.40 - 0.70 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Nickel, Ni 29 - 32 %
29 - 32 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si <= 0.25 %
<= 0.25 %
Sulfur, S <= 0.010 %
<= 0.010 %
Titanium, Ti 0.20 - 0.50 %
0.20 - 0.50 %