Universal Wire Works Commercially Pure (AMS 4951) Titanium Alloy Filler Metal

Category Metal , Nonferrous Metal , Titanium Alloy , Unalloyed/Modified Titanium
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works Commercially Pure (AMS 4951) Titanium Alloy Filler Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal commercially pure titanium is extremely versatile for applications requiring high temperature resistance together with resistance to many chemical reagents. Commercially pure (cp) titanium has many unique properties providing industry with answers to a host of equipment problems. CP titanium is available in sheet, strip, plate, bar, billet, tubing and wire, and is used in aircraft engine and airframe applications where tensile strength to weight ratios are important.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 345 MPa
50000 psi
Tensile Strength, Yield 172 MPa

@Strain 0.200 %
25000 psi

@Strain 0.200 %
Elongation at Break 35 %
35 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Hydrogen, H <= 0.0050 %
<= 0.0050 %
Iron, Fe <= 0.20 %
<= 0.20 %
Nitrogen, N <= 0.050 %
<= 0.050 %
Other <= 0.60 %
<= 0.60 %
Oxygen, O <= 0.18 %
<= 0.18 %
Titanium, Ti 98.885 - 100 %
98.885 - 100 %
As Remainder