Universal Wire Works 187 Copper-Nickel Alloy Welding Wire

Category Metal , Nonferrous Metal , Copper Alloy , Nickel Alloy
Manufacturer Universal Wire Works
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 187 Copper-Nickel Alloy Welding Wire.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy 187 is used for arc welding of wrought or cast 70/30, 80/20, and 90/10 copper nickel alloys to themselves or to each other. Alloy 187 can be used for welding the clad side of copper-nickel clad steel. Electrode sizes 3/32 and 1/8 diameter can be used in all positions, while the larger 5/32 and 3/16 diameter are used in the flat and horizontal positions. POWER SUPPLY DCRP.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 345 MPa
50000 psi
Elongation at Break 30 %
30 %
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.75 %
<= 0.75 %
Carbon, C <= 0.15 %
<= 0.15 %
Copper, Cu >= 62.1 %
>= 62.1 %
as balance
Iron, Fe <= 2.5 %
<= 2.5 %
Manganese, Mn <= 4.0 %
<= 4.0 %
Nickel, Ni >= 29 %
>= 29 %
Other <= 0.50 %
<= 0.50 %
Phosphorous, P <= 0.020 %
<= 0.020 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti <= 1.0 %
<= 1.0 %