CMW® ELKONIUM 63 Silver Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy
Manufacturer CMW Inc.
Trade Name ELKONIUM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONIUM 63 Silver Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ELKONIUM® 63 alloy contains small amounts of magnesium and nickel. It is recommended for low voltage, vibrating contact DC applications for minimizing metal transfer. It is used in automobile voltage regulators and electrical gauges. In a heat-treated condition the material is CMW D63X alloy, a high strength material used for contact spring arms.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 10.5 g/cc
0.379 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell 15T 60
60
annealed
80
80
cold worked
Tensile Strength, Ultimate 207 MPa
30000 psi
annealed
345 MPa
50000 psi
cold worked
Elongation at Break 7.0 %
7.0 %
cold worked
35 %
35 %
annealed
Component Elements Properties Metric English Comments
Magnesium, Mg 0.20 %
0.20 %
Nickel, Ni 0.20 %
0.20 %
Silver, Ag 99.6 %
99.6 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000230 ohm-cm
0.00000230 ohm-cm
75 % IACS