MetalTek AGMA CL A UNS C90800 Gear Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer MetalTek
Trade Name AGMA
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek AGMA CL A UNS C90800 Gear Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Copper-tin alloy with high tensile, yield and compressive strength as well as wear resistance.Applications: Worm gears, steel mill nutsInformation provided by MetalTekCast UNS C90800; Cast Grade C90800; Cast ASTM B427, B505
Mechanical Properties Metric English Comments
Hardness, Brinell 95
95
500 kg
Tensile Strength, Ultimate >= 345 MPa
>= 50000 psi
Tensile Strength, Yield >= 195 MPa
>= 28300 psi
Elongation at Break >= 12 %
>= 12 %
Component Elements Properties Metric English Comments
Copper, Cu 87.8 %
87.8 %
Phosphorous, P 0.20 %
0.20 %
Tin, Sn 12 %
12 %