Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 29.0 - 40.0 MPa | 4210 - 5800 psi | Average value: 34.4 MPa Grade Count:16 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Tensile Strength, Ultimate | 25.0 - 40.0 MPa | 3630 - 5800 psi | |
Alliance BIN-40 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 32.0 - 40.0 MPa | 4640 - 5800 psi | ASTM D638 |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 32.0 - 40.0 MPa | 4640 - 5800 psi | ASTM D638 |
Arkema Group VOLTALEF® 302 PCTFE VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 25.0 - 40.0 MPa | 3630 - 5800 psi | |
Alliance BIN-26 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 25.0 - 40.0 MPa | 3630 - 5800 psi | |
Alliance BIN-45 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 25.0 - 40.0 MPa | 3630 - 5800 psi | |
Alliance BIN-48 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 25.0 - 40.0 MPa | 3630 - 5800 psi | |
Alliance BIN-55 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 25.0 - 40.0 MPa | 3630 - 5800 psi | |
Alliance BIN-72 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 20.0 - 40.0 MPa | 2900 - 5800 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |
|||
Tensile Strength, Ultimate | 18.0 - 40.0 MPa @Temperature 60.0 - 120 °C |
2610 - 5800 psi @Temperature 140 - 248 °F |
Average value: 29.3 MPa Grade Count:1 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |