Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin  (discontinued **)

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature impact strength when blended with other polymers.Applications: Golf ball covers; Shoe heel counters/stiffeners; Bowling pins; Auto rub strips.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
Exxon Method
Melt Flow 1.6 g/10 min
1.6 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Ultimate 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 380 %
380 %
ASTM D638
Flexural Modulus 0.340 GPa
49.3 ksi
ASTM D790
Tensile Impact Strength 550 kJ/m²
262 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
Exxon Method
Vicat Softening Point 54.0 °C
129 °F
Rate B; ASTM D-1525
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved