Dow BETAMATE™ 1496 V Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Dow Chemical
Trade Name BETAMATE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow BETAMATE™ 1496 V Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BETAMATE™ 1496 V is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excellent after gelling) Readily pumped at elevated temperatures Excellent adhesion to automotive steels, including coated steels and pretreated aluminum Resistant to degradation and substrate corrosion on environmental aging Compatible with electro-coat paint process in uncured state Information provided by Dow
Physical Properties Metric English Comments
Density 1.15 - 1.21 g/cc
0.0415 - 0.0437 lb/in³
Solids Content >= 99 %
>= 99 %
Viscosity 500000 cP

@Shear Rate 1.00 1/s,
Temperature 40.0 °C
500000 cP

@Shear Rate 1.00 1/s,
Temperature 104 °F
cone/plate
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 32.0 MPa
4640 psi
ISO 527-1
Elongation at Break 15 %
15 %
ISO 527-1
Modulus of Elasticity 1.60 GPa
232 ksi
ISO 527-1
Adhesive Bond Strength 30.0 MPa

@Thickness 2.00 mm
4350 psi

@Thickness 0.0787 in
Lap Shear (25 x 10 x 0.2 mm) (CRS St 1203, 170°C/30); EN 1465
Peel Strength 4.00 kN/m
22.8 pli
T-Peel (CRS St 1203, 0.5mm)
28.0 kN/m
160 pli
Impact Peel
Thermal Properties Metric English Comments
Flash Point >= 150 °C
>= 302 °F
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 170 °C
0.500 hour

@Temperature 338 °F
60.0 min

@Temperature 155 °C
1.00 hour

@Temperature 311 °F