Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 2180 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 8.00 - 15.0 MPa

@Temperature 60.0 - 90.0 °C
1160 - 2180 psi

@Temperature 140 - 194 °F
Average value: 11.5 MPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Tensile Strength, Ultimate 6.00 - 15.0 MPa
870 - 2180 psi
ATG s.r.l. CO-ECO Epichlorohydrin Rubber
Tensile Strength, Ultimate 9.00 - 15.0 MPa
1310 - 2180 psi
Average value: 12.3 MPa Grade Count:3
Overview of materials for Very Low Density Polyethylene (VLDPE)
This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va..
Tensile Strength, Ultimate 12.0 - 15.0 MPa
1740 - 2180 psi
Dow Advanta® 3302 Specialty Elastomer  (discontinued **)
Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000..
Tensile Strength, Ultimate 12.0 - 15.0 MPa
1740 - 2180 psi
Dow Advanta® 3650 Specialty Elastomer  (discontinued **)
Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000..
Tensile Strength, Ultimate 9.00 - 15.0 MPa

@Temperature 60.0 - 90.0 °C
1310 - 2180 psi

@Temperature 140 - 194 °F
Average value: 12.0 MPa Grade Count:1
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..
Tensile Strength, Ultimate 5.00 - 15.0 MPa

@Temperature 60.0 - 90.0 °C
725 - 2180 psi

@Temperature 140 - 194 °F
Average value: 10.0 MPa Grade Count:1
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..
Copyright © lookpolymers.com All Rights Reserved