Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 8.00 - 15.0 MPa @Temperature 60.0 - 90.0 °C |
1160 - 2180 psi @Temperature 140 - 194 °F |
Average value: 11.5 MPa Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
Tensile Strength, Ultimate | 6.00 - 15.0 MPa | 870 - 2180 psi | |
ATG s.r.l. CO-ECO Epichlorohydrin Rubber |
|||
Tensile Strength, Ultimate | 9.00 - 15.0 MPa | 1310 - 2180 psi | Average value: 12.3 MPa Grade Count:3 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Ultimate | 12.0 - 15.0 MPa | 1740 - 2180 psi | |
Dow Advanta® 3302 Specialty Elastomer
(discontinued **) Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000.. |
|||
Tensile Strength, Ultimate | 12.0 - 15.0 MPa | 1740 - 2180 psi | |
Dow Advanta® 3650 Specialty Elastomer
(discontinued **) Advanta® specialty elastomers provides good fluid resistance and better high temperature performance than nitrile or HNBR and lower cost than fluoroelastomers. Available in two grades. ASTM D2000.. |
|||
Tensile Strength, Ultimate | 9.00 - 15.0 MPa @Temperature 60.0 - 90.0 °C |
1310 - 2180 psi @Temperature 140 - 194 °F |
Average value: 12.0 MPa Grade Count:1 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |
|||
Tensile Strength, Ultimate | 5.00 - 15.0 MPa @Temperature 60.0 - 90.0 °C |
725 - 2180 psi @Temperature 140 - 194 °F |
Average value: 10.0 MPa Grade Count:1 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |