Dart Drop, Total Energy 5.00 - 8.00 J
3.69 - 5.90 ft-lb
Average value: 6.79 J Grade Count:14
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..