Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 5.00 - 8.00 J | 3.69 - 5.90 ft-lb | Average value: 6.79 J Grade Count:14 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |