Material Notes:
Product Description: Exceed 2018HA is a metallocene Catalyzed ethylene-hexene copolymer. Films made from Exceed 2018HA have outstanding tensile, impact strength, and puncture. These superior strength properties, along with excellent drawability, makes this a very versatile packaging film resin. The higher melt index also makes this polymer ideally suited for blending into LDPE rich films. Availability: Africa & Middle East, Asia Pacific and EuropeAdditive:Antiblock: NoSlip: No Processing Aid: Yes Thermal Stabilizer: Yes Applications: Bag in BoxBarrier Food PackagingBlown Film Blown Stretch Film Bread BagsFood packagingForm Fill and Seal PackagingFreezer Film General PackagingHeavy Duty Bags Lamination Film Multilayer Packaging FilmOverwrap FilmPackaging FilmsPremium Trash BagsStand Up PouchesTrash Bags Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ExxonMobil method
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 8.96 MPa
1300 psi
ASTM D882
Film Tensile Strength at Yield, TD 8.96 MPa
1300 psi
ASTM D882
Film Elongation at Break, MD 590 %
590 %
ASTM D882
Film Elongation at Break, TD 700 %
700 %
ASTM D882
Elmendorf Tear Strength MD 330 g
330 g
ASTM D1922
Elmendorf Tear Strength TD 460 g
460 g
ASTM D1922
Dart Drop Test 670 g
1.48 lb
ASTM D1709
Film Tensile Strength at Break, MD 60.0 MPa
8700 psi
ASTM D882
Film Tensile Strength at Break, TD 55.8 MPa
8100 psi
ASTM D882
1% Secant Modulus, MD 165 MPa
24000 psi
ASTM D882
1% Secant Modulus, TD 179 MPa
26000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 243 °C
<= 469 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 37 %
37 %
ASTM D1003
Gloss 18 %
18 %
45°; ASTM D2457