Material Notes:
Westlake EF608 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compounding applications as a carrier for masterbatch or other concentrates.Application/UsesCompounding base resinColor concentratesAdditive masterbatchesFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.919 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 50.8 microns
2.00 mil
Melt Flow 9.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 575 %
575 %
ASTM D882
Film Elongation at Break, TD 730 %
730 %
ASTM D882
Dart Drop 3.74 g/micron
95.0 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 21.4 MPa
3100 psi
ASTM D882
Film Tensile Strength at Break, TD 15.9 MPa
2300 psi
ASTM D882
1% Secant Modulus, MD 152 MPa
22000 psi
ASTM D882
1% Secant Modulus, TD 179 MPa
26000 psi
ASTM D882
Processing Properties Metric English Comments
Melt Temperature 182 - 204 °C
360 - 400 °F
with BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.5
2.5
Descriptive Properties Value Comments
Process Film
Region US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved