Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, Unreinforced
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced combination of engineering properties characterized by high melt point; high strength and rigidity; good toughness; soft hand and good chemical resistance. This resin is especially useful in applications where high elongation, good clarity in thin sections and soft feel are required. Typical Applications/End Uses: Typical uses include packaging films, monofilaments, bristles, and extruded profiles.Availability:Asia PacificEuropeNorth America Additives: Heat Stabilizer Features: Gasoline ResistanceGeneral Purpose Good Chemical ResistanceGood ToughnessHeat StabilizedHigh Melt StabilityHigh Molecular WeightHigh RigidityHigh StrengthMedium ViscosityOil ResistantSolvent ResistantUses:FilmIndustrial ApplicationsMonofilamentsProfilesRodsSheetTubingVacuum Bagging FilmAppearance: Natural ColorForms: PelletsProcessing Method: ExtrusionInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Water Absorption 8.5 %

@Time 86400 sec
8.5 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.5 %
2.5 %
50% RH; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527-2
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527-2
Elongation at Break >= 200 %
>= 200 %
ISO 527-2
Elongation at Yield 30 %
30 %
ISO 527-2
Tensile Modulus 0.500 GPa
72.5 ksi
ISO 527-2
Flexural Strength 8.00 MPa
1160 psi
ISO 178
Flexural Modulus 0.250 GPa
36.3 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 180
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eU
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eA