Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, dry

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11, Cable Sheathing Grade
Manufacturer Suzhou Hipro Polymers
Trade Name Hiprolon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, dry.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hiprolon® 11ESNNHL P20 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact resistance, high burst pressure, low gasoline permeation, and good chemical resistance. It is widely used for auto fuel lines, air brake tubing, cable sheathing et al and meets ISO 7628, DIN 73378, DIN 74324 standards in automotive industry.Information provided by Suzhou Hipro Polymers Co. Ltd
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ISO 1183
Water Absorption 1.8 %
1.8 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ISO 527-1/-2
Tensile Modulus 0.500 GPa
72.5 ksi
ISO 527-1/-2
Thermal Properties Metric English Comments
Melting Point 187 °C
369 °F
ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °C
117 °F
ISO75-1/-2
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 190 - 250 °C
374 - 482 °F
Drying Temperature 80.0 - 90.0 °C
176 - 194 °F
Dry Time 4 hour
4 hour
Moisture Content <= 0.10 %
<= 0.10 %