Nylacast Moly Cast Nylon 6, MoS2 Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, MoS2 Filled
Manufacturer Nylacast
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylacast Moly Cast Nylon 6, MoS2 Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylacast Moly is part of the Cast Nylon 6 family. Its improved crystallization occurs by the addition of Molybdenum Disulphide. It includes MoS2, which is an extremely effective self dry lubricant which improves the properties of wear and abrasion resistances, combined with lower water absorption.Information provided by Nylacast Ltd.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
method A; ISO 1183:1987
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
Immersion; ISO 62:1999
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 82
80 - 82
ISO 868:2003
Tensile Strength, Yield 79.0 - 85.0 MPa
11500 - 12300 psi
Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 20 %
>= 20 %
Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 3.70 GPa
537 ksi
Type 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 110 MPa
16000 psi
1.5mm/min; ISO 178:2001
Flexural Modulus 3.20 GPa
464 ksi
1.5mm/min; ISO 178:2001
Compressive Strength 100 - 145 MPa
14500 - 21000 psi
Type B, 5mm/min; ISO 604:2002
Compressive Modulus 2.70 GPa
392 ksi
Type B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 5.39 kJ/m²
2.56 ft-lb/in²
Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.25

@Pressure 1.75 MPa
0.25

@Pressure 254 psi
31.4m/min
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Melting Point 223 °C
433 °F
Maximum Service Temperature, Air 170 °C
338 °F
Intermittent
105 °C

@Time 1.80e+7 sec
221 °F

@Time 5000 hour
Continuous
Minimum Service Temperature, Air -100 °C
-148 °F
Intermittent
-40.0 °C
-40.0 °F
Continuous
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093:1980-01
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093:1980-01
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
IEC 60250:1969-01
4.0

@Frequency 100 Hz
4.0

@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1:1998-01
Comparative Tracking Index 600 V
600 V
IEC 60112:2003-01
Descriptive Properties Value Comments
Color Black