Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cossa Polimeri ESTAPROP K 1280 T8 Polypropylene, 40% Mineral Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Mineral Reinforced
Manufacturer Cossa Polimeri S.r.L.
Trade Name ESTAPROP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cossa Polimeri ESTAPROP K 1280 T8 Polypropylene, 40% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP copolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
ASTM D 955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D 638
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D 638
Elongation at Break 30 %
30 %
ASTM D 638
Tensile Modulus 3.70 GPa
537 ksi
ASTM D 638
Flexural Modulus 3.50 GPa
508 ksi
ASTM D 790
Izod Impact, Notched 0.250 J/cm

@Temperature -20.0 °C
0.468 ft-lb/in

@Temperature -4.00 °F
ASTM D 638
0.300 J/cm

@Temperature 0.000 °C
0.562 ft-lb/in

@Temperature 32.0 °F
ASTM D 638
0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
136 °F
120°C/hr; ASTM D 648
Vicat Softening Point 75.0 °C

@Load 5.00 kg
167 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Users viewing this material also viewed the following: