Material Notes:
LNP* Thermocomp* DZ004 is a compound based on Polycarbonate resin containing Glass Fiber. Also known as Thermocomp DF-1004 M
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Tensile Modulus 3.70 GPa
537 ksi
50 mm/min; ASTM D638
Flexural Strength 96.0 MPa
13900 psi
ASTM D790
Flexural Modulus 3.50 GPa
508 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 11.42 J/cm
21.39 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 136 °C

@Thickness 3.20 mm
277 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 4.04e+16 - 5.90e+16 ohm-cm
4.04e+16 - 5.90e+16 ohm-cm
ASTM D257
Surface Resistance 3.09e+13 - 3.87e+13 ohm
3.09e+13 - 3.87e+13 ohm
ASTM D257
Dielectric Strength 24.3 kV/mm

@Thickness 1.60 mm
617 kV/in

@Thickness 0.0630 in
in air; ASTM D149
Dissipation Factor 0.0083

@Frequency 1.00e+6 Hz
0.0083

@Frequency 1.00e+6 Hz
ASTM D150