Mechanical Properties Metric English Comments
Tensile Modulus 14.2 GPa

@Temperature 23.0 °C
2060 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Crastin® SK608 BK509 PBT  (Unverified Data**)
Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 14.2 GPa
2060 ksi
ASTM D638
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH  (disco
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
Tensile Modulus 14.2 GPa
2060 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Tensile Modulus 14.2 GPa
2060 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific)
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Tensile Modulus 14.2 GPa
2060 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF0079SZ PA 66
LNP* THERMOCOMP* RF0079SZ is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Tensile Modulus 14.2 GPa
2060 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF0079SZ PA 66 (Asia Pacific)
LNP* Thermocomp* RF0079SZ is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Tensile Modulus 14.2 GPa
2060 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DX05042 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DX05042 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.
Tensile Modulus 14.2 GPa
2060 ksi
ISO 527
Polyram PlusTek PB318G9 Nylon 6 for Injection Molding, 45% Glass-fiber Reinforced, UV Stabilized
45% Glass-fiber reinforced Nylon 6, UV stabilized for injection molding applications.Information provided by Polyram.
Tensile Modulus 14.2 GPa
2060 ksi
ISO 527-1/-2
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)  (Unverified Data**)
45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
Tensile Modulus 14.2 GPa
2060 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6  (Unverified Data**)
45% Glass Reinforced Polyamide 6 Zytel 73G45 BK263 is a 45% glass fiber reinforced black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 14.2 GPa
2060 ksi
ISO 527
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..