Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH  (disco

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH  (disco.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, plus superior thermal performance to resist blistering during lead-free SMT processes. Color stability is enhanced compared to previous flame-retarded grades. Quick crystallization in water-cooled molds allows for fast cycle times using mold temperatures as low as 150°F (65°C).Information provided by Solvay Advanced Polymers
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.10 %
0.10 %
24 hours; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 178 MPa
25800 psi
ASTM D638
Elongation at Yield 1.7 %
1.7 %
ASTM D638
Tensile Modulus 14.2 GPa
2060 ksi
ASTM D638
Flexural Strength 257 MPa
37300 psi
ASTM D790
Flexural Modulus 14.1 GPa
2050 ksi
ASTM D790
Poissons Ratio 0.37
0.37
Shear Modulus 5.18 GPa
751 ksi
Calculated
Shear Strength 70.0 MPa
10200 psi
ASTM D732
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 326 °C
619 °F
ASTM D3418