SABIC Innovative Plastics LNP STAT-KON DX05042 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DX05042 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* DX05042 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 157 MPa
22800 psi
5 mm/min; ISO 527
Elongation at Break 2.1 %
2.1 %
5 mm/min; ISO 527
Tensile Modulus 14.2 GPa
2060 ksi
1 mm/min; ISO 527
Flexural Strength 223 MPa
32300 psi
2 mm/min; ISO 178
Flexural Modulus 11.3 GPa
1640 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 12.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
6.67 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 68.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
37.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
289 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 145 °C
293 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D257