DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zytel® 73G45 BK263 is a 45% glass fiber reinforced, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
DAM; ISO 1183
Filler Content 45 %
45 %
DAM
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Thickness 2.00 mm
0.0015 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Thickness 2.00 mm
0.0090 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa

@Temperature 23.0 °C
21000 psi

@Temperature 73.4 °F
50%RH; ISO 527
215 MPa

@Temperature 23.0 °C
31200 psi

@Temperature 73.4 °F
DAM; ISO 527
Elongation at Break 3.0 %

@Temperature 23.0 °C
3.0 %

@Temperature 73.4 °F
DAM; ISO 527
5.0 %

@Temperature 23.0 °C
5.0 %

@Temperature 73.4 °F
50%RH; ISO 527
Tensile Modulus 9.00 GPa

@Temperature 23.0 °C
1310 ksi

@Temperature 73.4 °F
50%RH; ISO 527
14.2 GPa

@Temperature 23.0 °C
2060 ksi

@Temperature 73.4 °F
DAM; ISO 527
Izod Impact, Notched (ISO) 17.0 kJ/m²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 180/1A
22.0 kJ/m²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 180/1A
Charpy Impact Unnotched 10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eU
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eU
Charpy Impact, Notched 1.90 J/cm²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
2.40 J/cm²

@Temperature 23.0 °C
11.4 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 9400 MPa

@Temperature 23.0 °C
1.36e+6 psi

@Temperature 73.4 °F
50%RH; ISO 899
Tensile Creep Modulus, 1000 hours 7300 MPa

@Temperature 23.0 °C
1.06e+6 psi

@Temperature 73.4 °F
50%RH; ISO 899
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 218 °C
424 °F
DAM; ISO 75-1/-2
Electrical Properties Metric English Comments
Comparative Tracking Index 500 V

@Temperature 23.0 °C
500 V

@Temperature 73.4 °F
DAM; IEC 60112
Processing Properties Metric English Comments
Melt Temperature 270 °C
518 °F
DAM; Optimum
260 - 280 °C
500 - 536 °F
DAM
Mold Temperature 70.0 - 120 °C
158 - 248 °F
DAM
100 °C
212 °F
DAM; optimum
Drying Temperature 80.0 °C
176 °F
DAM
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
DAM
Moisture Content <= 0.20 %
<= 0.20 %
DAM
Descriptive Properties Value Comments
Appearance Black Color
DAM
Drying Recommended Yes, if moisture content of resin exceeds recommended level
DAM
Features Chemical Resistance, Good
DAM
Fatigue Resistant
DAM
Fuel Resistant
DAM
Grease Resistant
DAM
Oil Resistant
DAM
Stiffness, High
DAM
Strength, High
DAM
Filler Glass fiber reinforcement
DAM
Forms Pellets
DAM
Generic Nylon 6
DAM
Material Status Current
DAM
Part Marking Code >PA6-GF45<
ISO 11469; DAM
Polymer Family Polyamide
DAM
Polymer Type PA6
DAM
Processing Method Injection Molding
DAM
Product Category Glass Reinforced Resins
DAM
Region Available - Global Yes
DAM
Resin Identification PA6-GF45
ISO 1043; DAM
RoHS Compliance Contact Manufacturer
DAM
Uses Appliance Components
DAM
Automotive Applications
DAM
Electrical/Electronic Applications
DAM
High Gloss Applications
DAM
Industrial Applications
DAM