Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
1.52 g/cc
0.0549 lb/in³
ISO 1183
Moisture Absorption 0.100 %
0.100 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
0.0023 cm/cm

@Time 86400 sec
0.0023 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ASTM D955
0.0052 cm/cm

@Time 86400 sec
0.0052 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 154 MPa
22300 psi
ISO 527
164 MPa
23800 psi
ASTM D638
Elongation at Break 7.2 %
7.2 %
ISO 527
7.3 %
7.3 %
ASTM D638
Tensile Modulus 14.2 GPa
2060 ksi
1 mm/min; ISO 527
22.06 GPa
3200 ksi
50 mm/min; ASTM D638
Flexural Strength 241 MPa
35000 psi
ASTM D790
250 MPa
36300 psi
ISO 178
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
11.7 GPa
1700 ksi
ISO 178
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.46 J/cm
12.1 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 39.0 kJ/m²
18.6 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 41.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 23.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.8 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
23.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
13.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 207 °C
405 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 201 °C
394 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
195 °C

@Thickness 3.20 mm
383 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved