Material Notes:
LNP* THERMOCOMP* RF0079SZ is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 154 MPa
22300 psi
ASTM D638
Elongation at Break 1.6 %
1.6 %
ASTM D638
Tensile Modulus 14.2 GPa
2060 ksi
50 mm/min; ASTM D638
Flexural Strength 234 MPa
33900 psi
ASTM D790
Flexural Modulus 12.41 GPa
1800 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.52 J/cm
10.3 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 235 °C

@Thickness 3.20 mm
455 °F

@Thickness 0.126 in
unannealed; ASTM D648