Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 14.2 GPa @Temperature 23.0 °C |
2060 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 14.2 GPa | 2060 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH
(disco AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Tensile Modulus | 14.2 GPa | 2060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Tensile Modulus | 14.2 GPa | 2060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific) LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Tensile Modulus | 14.2 GPa | 2060 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF0079SZ PA 66 LNP* THERMOCOMP* RF0079SZ is a compound based on Nylon 66 resin containing 35% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Tensile Modulus | 14.2 GPa | 2060 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RF0079SZ PA 66 (Asia Pacific) LNP* Thermocomp* RF0079SZ is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Tensile Modulus | 14.2 GPa | 2060 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX05042 PC (Europe-Africa-Middle East) LNP* Stat-kon* DX05042 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |
|||
Tensile Modulus | 14.2 GPa | 2060 ksi | ISO 527 |
Polyram PlusTek PB318G9 Nylon 6 for Injection Molding, 45% Glass-fiber Reinforced, UV Stabilized 45% Glass-fiber reinforced Nylon 6, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 14.2 GPa | 2060 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Tensile Modulus | 14.2 GPa | 2060 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6 Zytel 73G45 BK263 is a 45% glass fiber reinforced black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 14.2 GPa | 2060 ksi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 CF20 Polyamide 6 20% Carbon Fiber- Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |