Material Notes:
A CHEMICALLY COUPLED 35% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 210 MPa
30500 psi
ASTM-D638
Elongation at Break 2.0 %
2.0 %
ASTM-D638
Tensile Modulus 12.0 GPa
1740 ksi
ASTM-D790
Flexural Strength 305 MPa
44200 psi
ASTM-D790
Flexural Modulus 10.0 GPa
1450 ksi
ASTM-D790
Izod Impact, Notched 2.70 J/cm

@Temperature 23.0 °C
5.06 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ASTM-D648