EMS-Grivory Grivory® LVX-50H black 9230 PA12-GF50

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 50% Glass Fiber Filled
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® LVX-50H black 9230 PA12-GF50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilamid LVX-50H black 9230 is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and strengthExcellent impact and notched impact strengthExcellent UV, heat and chemical resistanceVery low moisture absorptionSuitable for repeated steam sterilizationGood flow characteristicsHigh molding precision, low warpage Grilamid LVX-50H black 9230 is especially suitable for complex structural parts in applications such as: Electronic devicesAutomotiveMechanical engineeringSafety componentsMedical devices and instrumentsSports & leisure goodsInformation provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183
Water Absorption 0.80 %
0.80 %
ISO 62
Moisture Absorption 0.400 %
0.400 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
conditioned; ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 12.0 GPa
1740 ksi
conditioned; ISO 527-1/-2
Charpy Impact Unnotched 8.50 J/cm²
40.4 ft-lb/in²
conditioned; ISO 179/1eU
8.50 J/cm²

@Temperature 30.0 °C
40.4 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 2.50 J/cm²
11.9 ft-lb/in²
conditioned; ISO 179/1eA
2.00 J/cm²

@Temperature 30.0 °C
9.52 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °C
194 - 248 °F
long term; EMS
150 °C
302 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 130 °C
266 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 55.0 kV/mm
1400 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Compressed air systems
Exterior
Fuel systems
Hydraulic systems
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Lighting
Mobile phones and other portable devices
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Medical devices
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved flowability and demoulding
Special Characteristics High impact or impact modified
Improved heat resistance
Improved UV resistance (outdoor use)