DuPont Performance Polymers Zytel® HTN FG52G35HSLR BK011 Polyphthalamide (PPA)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Zytel® HTN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN FG52G35HSLR BK011 Polyphthalamide (PPA)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 185 MPa
26800 psi
50%RH; ISO 527-1/-2
205 MPa
29700 psi
DAM; ISO 527-1/-2
Elongation at Break 2.2 %
2.2 %
DAM; ISO 527-1/-2
2.6 %
2.6 %
50%RH; ISO 527-1/-2
Tensile Modulus 12.0 GPa
1740 ksi
DAM; ISO 527-1/-2
12.0 GPa
1740 ksi
50%RH; ISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
DAM; ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
DAM; ISO 179/1eA
Descriptive Properties Value Comments
Additives Release agent
Delivery Form Pellets
Processing Injection Moulding
Regional Availability Europe
Near East/Africa
Special Characteristics Heat stabilised or stable to heat
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved