SABIC Innovative Plastics LNP LUBRICOMP KFI16 Acetal Copolymer (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP KFI16 Acetal Copolymer (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* KFI16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Silicone.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 125 MPa
18100 psi
5 mm/min; ISO 527
Elongation at Break 2.5 %
2.5 %
5 mm/min; ISO 527
Tensile Modulus 8.10 GPa
1170 ksi
1 mm/min; ISO 527
Flexural Strength 139 MPa
20200 psi
2 mm/min; ISO 178
Flexural Modulus 6.30 GPa
914 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
23.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 88.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
48.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af