Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.4 MPa
7600 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging VEO-184 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Oxford Polymers 802-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy
Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant
Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec..
Tensile Strength, Yield 52.4 - 79.3 MPa
7600 - 11500 psi
Average value: 63.6 MPa Grade Count:4
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum ..
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM Data
Americas Styrenics Styron® 663 Polystyrene  (discontinued **)
STYRON® 663 general purpose polystyrene resin is an additive free resin with excellent strength, clarity, and high heat resistance. When used unmodified for the manufacture of food contact articles..
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM Data
Americas Styrenics Styron® 685 Polystyrene  (discontinued **)
STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use..
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM Data
Americas Styrenics Styron® 685P Polystyrene  (discontinued **)
STYRON® 685P general purpose polystyrene resin is a high heat resin with good strength, moldability/processability, and excellent clarity. This resin is typically used in consumer electronic applic..
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Tensile Strength, Yield 52.4 MPa
7600 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Fittings M1015 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
I. Stern WC-103 General Purpose Crystal Polystyrene
Features:Good Processing CharacteristicsUL Classification 94 HBExcellent Water ClarityApplicationsExtrusion FoamDisplaysInformation provided by I. Stern & Co. Inc.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Global GP-110 High Impact Polystyrene
High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys
Tensile Strength, Yield 52.4 MPa
7600 psi
2.0 in/min; ASTM D638
LTL Color Compounds ColorFast® NY2115 Nylon 66
Super tough nylon 6,6 with excellent chemical resistance and ductilityAll information provided by LTL Color Compounders, Inc.
Tensile Strength, Yield 52.4 MPa

@Temperature 23.0 °C
7600 psi

@Temperature 73.4 °F
ASTM D638
IRPC Polimaxx Polene GP110 Polystyrene
APPLICATIONS: EXTRUSION SHEET, HOUSEHOLD PRODUCTS VACUUM SHEET , FOOD PACKAGING, TOY, SANITARY WARE, etc.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Techmer ES HiFill® ABS E GM5 LE 5% Glass Filled
Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Spartech Acrylloy 7 Acrylic Sheet
Description: Acrylic SheetInformation provided by Spartech.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Spartech Acrylloy F Acrylic Sheet
Description: Acrylic SheetInformation provided by Spartech.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Spartech Tuf-Glas Impact Modified Acrylic Sign Grade Sheet
Description: Sign Grade SheetInformation provided by Spartech.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Techmer ES HiFill® TPU GF20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Techmer ES Plastiblend® PC/PBT IM 5220 BK
Availability: North AmericaForms: PelletsAdditive: Impact Modifier and UV StabilizerFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D 638
Styrolution PS 1200/1201 GPPS
Extrusion / thermoforming foam sheetHigh melt strengthHigh StiffnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D 638
Styrolution PS 1290/1291 GPPS
Extrusion / thermoforming foam sheetLow residual styrene monomer contentHigh melt strength and stiffnessUL Classification 94 HB for 1290Information provided by Styrolution
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Techmer ES HiFill® PP GF/M35 CC BK 35% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Techmer ES Luriblend® PSU TL20
Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM 638
PlastxWorld CEVIAN® LMB10 Laser Markable Grade ABS
Black MarkingThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Total PSC 585 Polystyrene
Polystyrene 585 is a high molecular weight, low melt flow, crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. 585 also mak..
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Asahi Kasei Thermylene® P6-10FG-0600 10% Glass Fiber Reinforced, Heat Stabilized
Information provided by Asahi Thermofil