IRPC Polimaxx Polene GP110 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene GP110 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
APPLICATIONS: EXTRUSION SHEET, HOUSEHOLD PRODUCTS VACUUM SHEET , FOOD PACKAGING, TOY, SANITARY WARE, etc.
Physical Properties Metric English Comments
Melt Flow 1.7 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.7 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80

@Thickness 6.35 mm,
Temperature 23.0 °C
80

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D785
Tensile Strength, Yield 52.4 MPa

@Temperature 23.0 °C
7600 psi

@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 99.93 MPa

@Temperature 23.0 °C
14490 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 3.24 GPa

@Temperature 23.0 °C
469 ksi

@Temperature 73.4 °F
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C

@Thickness 6.35 mm
208 °F

@Thickness 0.250 in
ASTM D648
Vicat Softening Point 107 °C

@Load 1.00 kg,
Thickness 3.17 mm
225 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Processing Properties Metric English Comments
Processing Temperature 190 - 240 °C
374 - 464 °F
extrusion
210 - 240 °C
410 - 464 °F
injection