Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

I. Stern WC-103 General Purpose Crystal Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Extrusion Grade
Manufacturer I. Stern & Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF I. Stern WC-103 General Purpose Crystal Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Good Processing CharacteristicsUL Classification 94 HBExcellent Water ClarityApplicationsExtrusion FoamDisplaysInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Melt Flow 1.6 g/10 min
1.6 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Elongation at Yield 2.4 %
2.4 %
ASTM D638
Flexural Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 2.377 GPa
344.8 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ASTM D648
Vicat Softening Point 109 °C
228 °F
ASTM D1525
Flammability, UL94 HB
HB