Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PSC 585 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Total Atofina
Trade Name PSC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSC 585 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polystyrene 585 is a high molecular weight, low melt flow, crystal polystyrene. This polymer is tailored for extruded foam applications such as egg cartons, meat trays and food service. 585 also makes superior oriented polystyrene sheet.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 1.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Flexural Strength 97.9 MPa
14200 psi
ASTM D790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 107 °C
224 °F
ASTM D1525
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved