Global GP-110 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Global Polymers Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Global GP-110 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys
Physical Properties Metric English Comments
Melt Flow 1.7 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.7 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 79

@Thickness 6.35 mm
79

@Thickness 0.250 in
ASTM D785
Tensile Strength, Yield 52.4 MPa
7600 psi
ASTM D638
Flexural Yield Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 3.23 GPa
469 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 97.8 °C

@Thickness 6.35 mm
208 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Vicat Softening Point 107 °C
225 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Descriptive Properties Value Comments
Appearance Transparent
Forms Pellets
Users viewing this material also viewed the following: