Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 75.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 - 75.0 MPa
10200 - 10900 psi
Type 1B, 50mm/min; ISO 527-1/2:1993
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled)
This exceptional oil-loaded nylon features a complex blended oil lubrication system, uniformly distributed throughout the product, that guarantees constant performance over the whole service life. E..
Tensile Strength, Yield 50.0 - 75.0 MPa
7250 - 10900 psi
Injection; ISO 527
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
Tensile Strength, Yield 44.1 - 75.0 MPa
6400 - 10900 psi
Average value: 55.0 MPa Grade Count:12
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Tensile Strength, Yield 49.6 - 75.0 MPa
7200 - 10900 psi
Average value: 62.8 MPa Grade Count:97
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Tensile Strength, Yield 50.0 - 75.0 MPa

@Temperature 60.0 - 140 °C
7250 - 10900 psi

@Temperature 140 - 284 °F
Average value: 63.3 MPa Grade Count:1
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Yield 2.07 - 75.0 MPa
300 - 10900 psi
Average value: 27.9 MPa Grade Count:100
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..
Tensile Strength, Yield 21.0 - 75.0 MPa
3050 - 10900 psi
Average value: 43.2 MPa Grade Count:39
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
Copyright © lookpolymers.com All Rights Reserved