Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.5 MPa | 2400 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D638 |
LyondellBasell Petrothene® HR92953 Medium Density Polyethylene ApplicationsPETROTHENE HR 92953 is a medium density polyethylene-based resin designed for use as jacketing for communications cable, including CATV and FOC. HR 92953 has a nominal carbon black cont.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D638 |
Global TPO-45D TPO Grade Data provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 16.55 MPa | 2400 psi | ASTM D638 |
Lucent Polymers CPP-340 Polypropylene, 40% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D638 |
Multibase Multi-Flamâ„¢ 2903 LDPE Polyethylene Features:Flame RetardantHalogen Content, Low to NoneBlooming, None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D638 |
Techmer ES HiFill® PP GB60 60% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | >= 16.5 MPa | >= 2400 psi | ASTM D-882 |
Saint-Gobain Norton® T-200 Mechanical Grade PTFE Sheet (0.015" thick) Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate release sheets, .. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex APEX® 3202-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex APEX® 3302-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | 3; ASTM D412 |
Teknor Apex Flexalloy® 3501-70-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex Flexalloy® 9300-65 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D412 |
Teknor Apex APEX® 3300-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 20 PHR HAF Black (Typical) MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | at 2.0 in/min; ASTM D638 |
Chevron Phillips EA6740 Rubber Modified Polystyrene DescriptionChevron EA6740 is a high impact polystyrene material developed for packaging applications. Its processing characteristics make EA6740 excellent for extrusion and deep-draw thermoforming... |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 6710 Moldings & Extrusions Flexible PVC Clear extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | >= 16.5 MPa | >= 2400 psi | ASTM D638 |
Buckeye Polymers BP FLEX D5718 TU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 01560 Plenum Flexible PVC CAT 5 rated plenum jacket.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 8802 Moldings & Extrusions Flexible PVC General purpose extrusion compound designed for use in weatherstrips, screen splines and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 8810 Moldings & Extrusions Flexible PVC Low gravity extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required. Exhibits good flex whitening resistance.Information pro.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® IT 37-035 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledUV StabilizedApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First Choic.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 22871 Coax & Telecom Flexible PVC Non-lead, category 5 flexible CMR jacket over HDPE inners.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 18840 Wire & Cable Flexible PVC Non-lead stabilized 105C jacket compound for use in SPTO, SJTO and SVTO applications. Best suited for 30 mil walls and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |
|||
Tensile Strength, Yield | 16.5 MPa | 2400 psi | ASTM D-638 |
Axiall 286FR Moldings & Extrusions Flexible PVC 105C plug molding compound. UL recognized component for 94 V-2 in all colors (0.75 mm min. thickness). UL QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axiall .. |
|||
Tensile Strength, Yield | 16.5 - 150 MPa | 2400 - 21800 psi | Average value: 111 MPa Grade Count:7 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |