Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Thanecure® ZM

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR Thanecure® ZM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.THANECURE ZM activator is a partial complex of zinc chloride and MBTS which develops a fast rate of cure in MILLATHANE® HT. The improvement in the rate of cure in MILLATHANE HT imparted by the addition of THANECURE ZM is shown below. The addition of the THANECURE ZM improves the compression set resistance and does not detract from the outstanding abrasion and tear resistance of its vulcanizates.All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
Tensile Strength, Yield 16.5 MPa
2400 psi
Elongation at Yield 464 %
464 %
100% Modulus 0.00400 GPa
0.580 ksi
200% Modulus 0.008170 GPa
1.185 ksi
300% Modulus 0.01218 GPa
1.767 ksi
Tear Strength 41.0 kN/m
234 pli
Die C
Compression Set 68 %

@Temperature 70.0 °C,
Time 79200 sec
68 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 34.0 min

@Temperature 160 °C
0.567 hour

@Temperature 320 °F
Press cured
Descriptive Properties Value Comments
DIN Abrasion (mm³) 107