Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flamâ„¢ 2903 LDPE Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Multibase
Trade Name Multi-Flam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flamâ„¢ 2903 LDPE Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Flame RetardantHalogen Content, Low to NoneBlooming, None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ASTM D792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.5 MPa
2400 psi
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Flexural Modulus 0.214 GPa
31.0 ksi
ASTM D790
Izod Impact, Notched 4.97 J/cm
9.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-2
V-2
0.125 in
V-2
V-2
0.0625 in
Users viewing this material also viewed the following: