Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Synprene® IT 37-035 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® IT 37-035 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledUV StabilizedApplications:General PurposeMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
10 Sec; ASTM D2240
Tensile Strength, Yield 16.5 MPa
2400 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
15.0 MPa

@Strain 300 %
2170 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 500 %
500 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 94.7 kN/m
540 pli
Die C (graves), 20 in/min; ASTM D624