Axiall 8810 Moldings & Extrusions Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 8810 Moldings & Extrusions Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low gravity extrusion compound especially formulated for extruded T-moldings and other shapes where uniform flow through the die is required. Exhibits good flex whitening resistance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.28 g/cc
1.24 - 1.28 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 84
78 - 84
delayed; ASTM D-2240
Tensile Strength, Yield 16.5 MPa
2400 psi
ASTM D-638
Elongation at Yield 350 %
350 %
ASTM D-638
100% Modulus 0.008791 GPa
1.275 ksi
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F