Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PA66GM38BK Nylon 66, 38% Glass/Mineral Fiber Filled
Information provided by Niche Polymer
Izod Impact, Unnotched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PPHM15BK Homopolymer PP
Information provided by Niche Polymer
Izod Impact, Unnotched 0.427 J/cm

@Thickness 3.17 mm
0.800 ft-lb/in

@Thickness 0.125 in
ASTM D256
Niche Polymer PPHM6BK Homopolymer PP
Information provided by Niche Polymer
Izod Impact, Unnotched 0.427 - 9.08 J/cm
0.800 - 17.0 ft-lb/in
Average value: 5.03 J/cm Grade Count:32
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..