Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Izod Impact, Unnotched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 3101-25 Polyester BMC Premi-Glas® 3101-25 is a 25% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL .. |
|||
Izod Impact, Unnotched | 6.86 J/cm | 12.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP FARADEX NS0031 PC+ABS (Asia Pacific) Faradex NS0031 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel. Added features of this material include: EMI/RFI Shiel.. |
|||
Izod Impact, Unnotched | 6.90 - 9.10 J/cm | 12.9 - 17.0 ft-lb/in | Average value: 7.77 J/cm Grade Count:3 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Izod Impact, Unnotched | 6.89 J/cm | 12.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36P PC LNP* Lubricomp* DFL36P is a compound based on Polycarbonate containing 30% Glass Fiber 15% PTFE. Added features include: Exceptional Processing. Internally Lubricated. |
|||
Izod Impact, Unnotched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf.. |
|||
Izod Impact, Unnotched | 6.86 J/cm | 12.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12 LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Unnotched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 LNP LUBRILOY* RF206 is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material includes: Wear Resistant. |
|||
Izod Impact, Unnotched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY RF206AXH PA 66 LNP LUBRILOY* RF206AXH is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Unnotched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Izod Impact, Unnotched | 6.90 J/cm @Thickness 3.18 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi.. |
|||
Izod Impact, Unnotched | 6.88 J/cm | 12.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 (Asia Pacific) LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |
|||
Izod Impact, Unnotched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 130 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Izod Impact, Unnotched | 6.90 J/cm @Thickness 3.18 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta.. |
|||
Izod Impact, Unnotched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
Chevron Phillips Xtel® XK2340 Polyphenylene Sulfide Alloy Black Polyphenylene Sulfide AlloyXtel™ XK2340 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength with an unique blend of toughness and.. |
|||
Izod Impact, Unnotched | 6.88 J/cm | 12.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP IX04513C PA 6/12 LNP THERMOCOMP* IX04513C is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Clean Compounding System. |
|||
Izod Impact, Unnotched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Triloy® 210N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantHeat resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |