Mechanical Properties Metric English Comments
Izod Impact, Unnotched 8.01 - 16.0 J/cm
15.0 - 30.0 ft-lb/in
Average value: 10.9 J/cm Grade Count:3
Overview of materials for Polyphenylene Ether, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values ..
Izod Impact, Unnotched 5.34 - 16.0 J/cm
10.0 - 30.0 ft-lb/in
Average value: 8.90 J/cm Grade Count:3
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
Izod Impact, Unnotched 2.67 - 16.0 J/cm
5.00 - 30.0 ft-lb/in
Average value: 5.32 J/cm Grade Count:64
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Izod Impact, Unnotched 2.14 - 16.0 J/cm
4.00 - 30.0 ft-lb/in
Average value: 8.37 J/cm Grade Count:15
Overview of materials for Fluorocarbon ETFE, with Glass or Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE, with Glass or Carbon Fiber Filler". Each property range of values reported is minimum..
Izod Impact, Unnotched 1.23 - 16.0 J/cm
2.30 - 30.0 ft-lb/in
Average value: 11.1 J/cm Grade Count:51
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Izod Impact, Unnotched 5.34 - 16.0 J/cm
10.0 - 30.0 ft-lb/in
Average value: 9.65 J/cm Grade Count:13
Overview of materials for Nylon 6, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria..
Izod Impact, Unnotched 0.801 - 16.0 J/cm
1.50 - 30.0 ft-lb/in
Average value: 7.99 J/cm Grade Count:66
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..
Izod Impact, Unnotched 2.40 - 16.0 J/cm
4.50 - 30.0 ft-lb/in
Average value: 6.99 J/cm Grade Count:10
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Izod Impact, Unnotched 4.27 - 16.0 J/cm
8.00 - 30.0 ft-lb/in
Average value: 10.5 J/cm Grade Count:7
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Izod Impact, Unnotched 3.74 - 16.0 J/cm
7.00 - 30.0 ft-lb/in
Average value: 9.28 J/cm Grade Count:13
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini..