Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyphenylene Ether, PTFE Filled

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, PTFE Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyphenylene Ether, PTFE Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.11 - 1.43 g/cc
0.0401 - 0.0517 lb/in³
Average value: 1.21 g/cc Grade Count:7
Water Absorption 0.0600 - 0.200 %
0.0600 - 0.200 %
Average value: 0.124 % Grade Count:5
Linear Mold Shrinkage 0.00200 - 0.0100 cm/cm
0.00200 - 0.0100 in/in
Average value: 0.00671 cm/cm Grade Count:7
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 39.6 - 115 MPa
5750 - 16700 psi
Average value: 57.3 MPa Grade Count:7
Elongation at Break 1.00 - 10.0 %
1.00 - 10.0 %
Average value: 7.30 % Grade Count:5
Modulus of Elasticity 1.93 - 13.0 GPa
280 - 1890 ksi
Average value: 4.01 GPa Grade Count:7
Flexural Yield Strength 69.0 - 170 MPa
10000 - 24700 psi
Average value: 89.8 MPa Grade Count:7
Flexural Modulus 2.07 - 11.0 GPa
300 - 1600 ksi
Average value: 3.68 GPa Grade Count:7
Izod Impact, Notched 0.590 - 1.17 J/cm
1.11 - 2.20 ft-lb/in
Average value: 0.950 J/cm Grade Count:5
Izod Impact, Unnotched 8.01 - 16.0 J/cm
15.0 - 30.0 ft-lb/in
Average value: 10.9 J/cm Grade Count:3
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 116 - 121 °C
240 - 250 °F
Average value: 119 °C Grade Count:3
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:5
Processing Properties Metric English Comments
Melt Temperature 249 - 316 °C
480 - 601 °F
Average value: 284 °C Grade Count:7
Mold Temperature 65.6 - 121 °C
150 - 250 °F
Average value: 94.8 °C Grade Count:7
Drying Temperature 93.3 - 121 °C
200 - 250 °F
Average value: 104 °C Grade Count:7
Moisture Content 0.100 %
0.100 %
Average value: 0.100 % Grade Count:3
Dew Point -17.8 °C
0.000 °F
Average value: -17.8 °C Grade Count:3
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:3