Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend , Nylon
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.900 - 1.15 g/cc
0.0325 - 0.0415 lb/in³
Average value: 1.06 g/cc Grade Count:60
Filler Content 8.00 - 9.00 %
8.00 - 9.00 %
Average value: 8.33 % Grade Count:3
Water Absorption 0.200 - 6.00 %
0.200 - 6.00 %
Average value: 2.17 % Grade Count:28
Moisture Absorption at Equilibrium 1.10 - 2.00 %
1.10 - 2.00 %
Average value: 1.54 % Grade Count:26
Water Absorption at Saturation 2.00 - 4.30 %
2.00 - 4.30 %
Average value: 3.40 % Grade Count:6
Linear Mold Shrinkage 0.00450 - 0.0110 cm/cm
0.00450 - 0.0110 in/in
Average value: 0.00776 cm/cm Grade Count:43
Linear Mold Shrinkage, Transverse 0.00600 - 0.0140 cm/cm
0.00600 - 0.0140 in/in
Average value: 0.00811 cm/cm Grade Count:18
Melt Flow 1.00 - 64.2 g/10 min
1.00 - 64.2 g/10 min
Average value: 15.1 g/10 min Grade Count:38
Mechanical Properties Metric English Comments
Hardness, Rockwell R 69.0 - 116
69.0 - 116
Average value: 99.2 Grade Count:23
Hardness, Shore D 64.0
64.0
Average value: 64.0 Grade Count:3
Tensile Strength, Ultimate 30.0 - 63.8 MPa
4350 - 9250 psi
Average value: 42.6 MPa Grade Count:34
Tensile Strength, Yield 27.0 - 55.0 MPa
3920 - 7980 psi
Average value: 39.8 MPa Grade Count:38
64.0 - 64.0 MPa

@Temperature -40.0 - -40.0 °C
9280 - 9280 psi

@Temperature -40.0 - -40.0 °F
Average value: 64.0 MPa Grade Count:1
Elongation at Break 3.10 - 230 %
3.10 - 230 %
Average value: 81.5 % Grade Count:54
Elongation at Yield 2.90 - 110 %
2.90 - 110 %
Average value: 8.94 % Grade Count:27
4.80 - 4.80 %

@Temperature -40.0 - -40.0 °C
4.80 - 4.80 %

@Temperature -40.0 - -40.0 °F
Average value: 4.80 % Grade Count:1
Modulus of Elasticity 0.900 - 3.50 GPa
131 - 508 ksi
Average value: 1.83 GPa Grade Count:35
Flexural Yield Strength 39.3 - 108 MPa
5700 - 15700 psi
Average value: 67.5 MPa Grade Count:42
Flexural Modulus 0.814 - 3.00 GPa
118 - 435 ksi
Average value: 1.84 GPa Grade Count:43
Izod Impact, Notched 0.588 J/cm - NB
1.10 ft-lb/in - NB
Average value: 6.34 J/cm Grade Count:33
0.5339 - 2.50 J/cm

@Temperature -40.0 - 0.000 °C
1.000 - 4.68 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 1.05 J/cm Grade Count:10
0.5339 - 2.50 J/cm

@Thickness 3.17 - 6.35 mm
1.000 - 4.68 ft-lb/in

@Thickness 0.125 - 0.250 in
Average value: 1.05 J/cm Grade Count:10
Izod Impact, Notched (ISO) 7.00 - 81.0 kJ/m²
3.33 - 38.5 ft-lb/in²
Average value: 54.6 kJ/m² Grade Count:12
5.00 - 57.0 kJ/m²

@Temperature -40.0 - -30.0 °C
2.38 - 27.1 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 17.3 kJ/m² Grade Count:7
Izod Impact, Unnotched (ISO) 100 - 160 kJ/m²
47.6 - 76.1 ft-lb/in²
Average value: 120 kJ/m² Grade Count:3
55.0 - 60.0 kJ/m²

@Temperature -30.0 - -30.0 °C
26.2 - 28.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 57.5 kJ/m² Grade Count:2
Charpy Impact Unnotched 15.0 J/cm² - NB
71.4 ft-lb/in² - NB
Average value: 15.2 J/cm² Grade Count:21
0.600 J/cm² - NB

@Temperature -30.0 - -30.0 °C
2.86 ft-lb/in² - NB

@Temperature -22.0 - -22.0 °F
Average value: 4.09 J/cm² Grade Count:21
Charpy Impact, Notched 0.600 - 8.50 J/cm²
2.86 - 40.5 ft-lb/in²
Average value: 5.66 J/cm² Grade Count:27
0.600 - 5.50 J/cm²

@Temperature -30.0 - -30.0 °C
2.86 - 26.2 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.58 J/cm² Grade Count:17
Puncture Energy 38.0 - 40.0 J
28.0 - 29.5 ft-lb
Average value: 39.5 J Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 0.650 - 119 µm/m-°C
0.361 - 66.1 µin/in-°F
Average value: 92.7 µm/m-°C Grade Count:21
CTE, linear, Transverse to Flow 1.00 - 127 µm/m-°C
0.556 - 70.6 µin/in-°F
Average value: 101 µm/m-°C Grade Count:10
Specific Heat Capacity 2.20 J/g-°C
0.526 BTU/lb-°F
Average value: 2.20 J/g-°C Grade Count:4
Thermal Conductivity 0.145 W/m-K
1.01 BTU-in/hr-ft²-°F
Average value: 0.145 W/m-K Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 190 °C
176 - 374 °F
Average value: 102 °C Grade Count:34
Deflection Temperature at 1.8 MPa (264 psi) 51.7 - 110 °C
125 - 230 °F
Average value: 74.1 °C Grade Count:52
Vicat Softening Point 91.0 - 245 °C
196 - 473 °F
Average value: 130 °C Grade Count:32
UL RTI, Electrical 60.0 - 110 °C
140 - 230 °F
Average value: 76.7 °C Grade Count:6
UL RTI, Mechanical with Impact 60.0 - 65.0 °C
140 - 149 °F
Average value: 61.7 °C Grade Count:6
UL RTI, Mechanical without Impact 60.0 - 105 °C
140 - 221 °F
Average value: 75.0 °C Grade Count:6
Flammability, UL94 HB
HB
Grade Count:34
Glow Wire Test 650 °C
1200 °F
Average value: 650 °C Grade Count:3
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+10 - 9.70e+15 ohm-cm
1.00e+10 - 9.70e+15 ohm-cm
Average value: 6.90e+14 ohm-cm Grade Count:32
Surface Resistance 1.00e+13 - 8.30e+15 ohm
1.00e+13 - 8.30e+15 ohm
Average value: 1.32e+15 ohm Grade Count:22
Dielectric Constant 2.90 - 6.70
2.90 - 6.70
Average value: 3.66 Grade Count:32
Dielectric Strength 15.0 - 41.0 kV/mm
380 - 1040 kV/in
Average value: 30.1 kV/mm Grade Count:25
Dissipation Factor 0.00770 - 0.100
0.00770 - 0.100
Average value: 0.0376 Grade Count:30
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:15
Processing Properties Metric English Comments
Nozzle Temperature 216 - 260 °C
420 - 500 °F
Average value: 249 °C Grade Count:4
Melt Temperature 204 - 280 °C
400 - 536 °F
Average value: 250 °C Grade Count:28
Mold Temperature 10.0 - 93.0 °C
50.0 - 199 °F
Average value: 68.8 °C Grade Count:25
Injection Velocity 40.0 - 65.0 mm/sec
1.57 - 2.56 in/sec
Average value: 47.7 mm/sec Grade Count:13
Drying Temperature 85.0 - 88.0 °C
185 - 190 °F
Average value: 87.3 °C Grade Count:4
Moisture Content 0.150 - 0.350 %
0.150 - 0.350 %
Average value: 0.250 % Grade Count:3
Dew Point -29.0 °C
-20.2 °F
Average value: -29.0 °C Grade Count:3