Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.40 - 1.70 J/cm² | 6.66 - 8.09 ft-lb/in² | ISO 11542-2 |
Okulen® 1000 PE-UHMW, UV - stabilized OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Charpy Impact Unnotched | 0.600 - 1.70 J/cm² | 2.86 - 8.09 ft-lb/in² | Average value: 1.12 J/cm² Grade Count:5 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 1.09 - 1.70 J/cm² | 5.19 - 8.09 ft-lb/in² | Average value: 1.38 J/cm² Grade Count:3 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact Unnotched | 1.10 - 1.70 J/cm² | 5.24 - 8.09 ft-lb/in² | ISO 179 |
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,.. |
|||
Charpy Impact Unnotched | 1.30 - 1.70 J/cm² | 6.19 - 8.09 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Charpy Impact Unnotched | 1.70 - 1.70 J/cm² @Temperature -40.0 - -20.0 °C |
8.09 - 8.09 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.70 J/cm² Grade Count:1 |
Overview of materials for Polypropylene with Glass Fiber + Bead Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + Bead Filler". Each property range of values reported is minimum and max.. |