Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.06 - 2.12 J/cm | 1.99 - 3.97 ft-lb/in | |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |