Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON DX03550 PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DX03550 PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* DX03550 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Tensile Modulus 2.75 GPa
399 ksi
50 mm/min; ASTM D638
Flexural Strength 96.0 MPa
13900 psi
ASTM D790
Flexural Modulus 2.75 GPa
399 ksi
ASTM D790
Izod Impact, Notched 1.06 J/cm
1.99 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 129 °C

@Thickness 3.20 mm
264 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10000 - 1.00e+7 ohm-cm
10000 - 1.00e+7 ohm-cm
ASTM D257
Surface Resistance 10000 - 1.00e+7 ohm
10000 - 1.00e+7 ohm
ASTM D257
Copyright © lookpolymers.com All Rights Reserved