Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.640 - 0.960 J/cm @Thickness 6.35 mm |
1.20 - 1.80 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.440 - 0.961 J/cm | 0.824 - 1.80 ft-lb/in | Average value: 0.714 J/cm Grade Count:13 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.400 - 0.960 J/cm @Temperature -40.0 - -29.0 °C |
0.749 - 1.80 ft-lb/in @Temperature -40.0 - -20.2 °F |
Average value: 0.620 J/cm Grade Count:3 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.750 - 0.960 J/cm | 1.41 - 1.80 ft-lb/in | Average value: 0.873 J/cm Grade Count:3 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.690 - 0.960 J/cm @Thickness 6.35 mm |
1.29 - 1.80 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ NL-10GF/15TF Nylon 6/12 - 10% Glass Fiber - 15% PTFE Flock
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.747 - 0.961 J/cm | 1.40 - 1.80 ft-lb/in | ASTM D256 |
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6 NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Izod Impact, Notched | 0.747 - 0.961 J/cm | 1.40 - 1.80 ft-lb/in | ASTM D256 |
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6 NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Izod Impact, Notched | 0.290 - 0.961 J/cm | 0.543 - 1.80 ft-lb/in | Average value: 0.565 J/cm Grade Count:80 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Notched | 0.690 - 0.960 J/cm @Thickness 6.35 mm |
1.29 - 1.80 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ ES-20GF/08T Polyethersulfone - 20% Glass Fiber And PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.590 - 0.960 J/cm @Thickness 6.35 mm |
1.11 - 1.80 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ MP-000/10T Modified PPO - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.160 - 0.961 J/cm | 0.300 - 1.80 ft-lb/in | Average value: 0.484 J/cm Grade Count:22 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Izod Impact, Notched | 0.641 - 0.961 J/cm | 1.20 - 1.80 ft-lb/in | Average value: 0.770 J/cm Grade Count:7 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |